BeStar FT-50T-0.87A1W130 User Manual

Page 1
SPECIFICATION
FOR PIEZO ELECTRIC BUZZER
Customer Customer P/N Date Page
TOTAL PAGE
11 Mar. 09
01 of 08
08
www.be-star.com
Model Name
Product No. Issue No. Issue Date
FT-50T-0.87A1W130
BS/TEY01.228A
09/03/11
Approval
1.Electrical characteristics
2.Dimension
3.Measuring Method
4."Pull off"force between silver and ceramic layer
5.Notice
6.Reliability Test
7.Packing
Drawn by
Checked by
Approved by
Customer approved
BESTAR ELECTRONICS INDUSTRY CO.,LTD
No.199 HuangHe West Road.New district,ChangZhou,JiangSu Province,P.R.China
Tel: +86 519 88222567 Fax: +86 519 88222551
E-mail:wu@be-star.com http://www.be-star.com
Page 2
FT-50T-0.87A1W130
46 5
23 1
H
H
1.Electrical characteristics
G
F
E
No. Item
1.
2.
3.
4.
5.
Resonant Frequency
Resonant Impedance
Static Capacitance
Insulation Resistance
Input Voltage
"Pull off"force between
6.
silver and ceramic layer (horizontally)
Specification Condition
The resonant frequency
0.87 ± 0.25KHz
is suitable for piezo
element with wire The resonant Impedance
3000 ohm max
is suitable only for piezo
element without wire
C:40±30%nF
at 120Hz
The Insulation esistance
Min.200M ohm
is suitable only for piezo
element without wire
30 Vp-p(at least)
20N min
G
F
E
"Pull off"force between
D
and shall not be used in whole or in part without its written content
7.
8.
9.
This print and information there in are proprietary to Bestar Electronics Industry Co., Ltd.
10.
C
B
A
A
Rev.
11.
09/03/11
Date
silver and ceramic
layer (vertically) Operating Temperature
Storage Temperature Lead Wire
Metallic supporter
汤浩君
Drawn
56
Note
2.5N min
-20...+60°C
-30...+70°C 130×3×3
Brass
Date: Drawn by: Checked by: Approved by:
www.be-star.com wu@be-star.com
4
09/03/11
汤浩君 耿 亚
李红元
3
Yellow (+) Blue (-)
FT-50T-0.87A1W130
Piezo Ceramic Element
BDRG NO: BS/TEY01.228A
2
D
C
B
A
Page:02 of 08
1
Page 3
6 5 4 3
FT-50T-0.87A1W130
12
H
H
2.Dimension
0.44±0.1
G
Ø50±0.1
0.2±0.03
Ø25±0.5
130±10
F
Yellow
Blue
3 ±1
E
G
F
E
UL1571 #24AWG
D
and shall not be used in whole or in part without its written content
Notes:
D
1.Element shall be free from obvious contamination,deep scratches and metal deformation
This print and information there in are proprietary to Bestar Electronics Industry Co., Ltd.
2.Edge of solder point shall be 1.5mm minimum from edge of brass.
3.Bonding glue should not exude beyound 1.0mm of the ceramic edge
4.Tolerance of concentricity between metal disc and ceramic shall be within 1.0mm
C
B
C
B
Date: Drawn by:
A
A
Rev.
09/03/11
Date
6
汤浩君
Drawn
Note
5
Checked by: Approved by:
www.be-star.com wu@be-star.com
4
09/03/11
汤浩君 耿 亚
李红元
3
FT-50T-0.87A1W130
Piezo Ceramic Element
BDRG NO: BS/TEY01.228A
A
Page:03 of 08
12
Page 4
6 5 4 3
FT-50T-0.87A1W130
H
3.Measuring Method
3.1.Resonant Frequency/Resonant Impedance piezoelectric diaphragm shall be clamped at a node point as shown in following figure to be free from any mechanical stress,and measured its resonant frequency and resonant impedance by using
2 1
H
G
F
E
D
YW2788 synthesis parameter test apparatus or equivalent
3.2.Capacitance: An electrostatic capacity capacitance shall be measured at 120Hz by using LCR meter, such as DF2812A LCR numerical bridge or equivalent.the part shall be clamped at the node .
G
F
E
D
and shall not be used in whole or in part without its written content
This print and information there in are proprietary to Bestar Electronics Industry Co., Ltd.
3.3.Insulation Resistance: An insulation resistance shall be measured by using an insulation resistance meter,suach as DF2863 insulation resistance meter.
C
B
09/03/11
汤浩君 耿
李红元
3
FT-50T-0.87A1W130
Piezo Ceramic Element
BDRG NO: BS/TEY01.228A
2 1
Page:04 of 08
09/03/11
A
Rev.
Date Drawn
6 5
汤浩君
Note
Date: Drawn by: Checked by: Approved by:
www.be-star.com wu@be-star.com
4
C
B
AA
Page 5
6 5 4 3 2 1
FT-50T-0.87A1W130
H
4."Pull off"force between silver and ceramic layer
Note:
4.1 Lead wire (UL 1571 #24AWG)to be soldered on the silver by handsoldering
H
G
at 300 10°C duration 2 0.5 sec
G
4.2.a Pull force by houizontal direction is 20N
4.2.b Pull force by vertical direction is 2.5N
Lead Wire
Lead Wire
F
E
(horizontally)
FIG.1 Direction of Lead Wire
FIG.2 Direction of Lead Wire
(vertically)
F
E
5. Notice
5.1 The products mustn't be washed
5.2 Storage Condition
D
and shall not be used in whole or in part without its written content
This print and information there in are proprietary to Bestar Electronics Industry Co., Ltd.
C
B
The products should be stored in the room ,where the temperature/humidity is stable. And avoid such places where there are large temperature changes. Please store the
products at the following conditions:
Temperature: -10 to + 40°C Humidity: 15 to 85% R.H.
5.3 Expire Date on Storage
Expire date (Shelf life) of the products is six months after deliveried under the conditions of a
sealed and an unopened package. Please use the products within six months after deliveried. If you store the products for a long time (more than six months), use carefully because the products may be degraded in the solderability and/or rusty.Please confirm solderability and characteristics for the products regularly.
5.4 Notice on Product Storage
(1) Please do not store the products in a chemical atmosphere (Acids, Alkali, Bases, Organic
gas, Sulfides and so on), because the characteristics may be reduced at quality, and/or be d-
egraded in the solderability due to the storage in a chemical atmosphere. (2) Please use the products immediately after the package is opened, because the character­istics may be reduced at quality, and/or be degraded in the solderability due to storage under
the poor condition. (3) Please do not drop the products to avoid cracking of ceramic element.
D
C
B
Date: Drawn by:
A
A A
Rev.
09/03/11
Date
6
汤浩君
Drawn
Note
5
Checked by: Approved by:
www.be-star.com wu@be-star.com
4
09/03/11
汤浩君 耿
李红元
3 2 1
FT-50T-0.87A1W130
Piezo Ceramic Element
BDRG NO: BS/TEY01.228A
Page:05 of 08
Page 6
6 5 4 3 2
FT-50T-0.87A1W130
1
H
H
6. Reliability test
6.1 Life test at high temperature Temperature +70°C Duration 96hrs
6.2 Life test at low temperature
G
F
E
D
and shall not be used in whole or in part without its written content
This print and information there in are proprietary to Bestar Electronics Industry Co., Ltd.
C
Temperature -30°C Duration 96hrs
6.3 Temperature cycle test Cycles 5
-30
30min
+20
15min
+70
30min
+20
15min
6.4 Humidity cycle test Cycles 5
65 90-95% RH
2590-95% RH
10h 1h 1h
12h
All these tests above should be measured after leaving normal temperature for 2hrs.
6.5 Vibration Test Vibration Frequency 10~55Hz Amplitude 1.53mm Direction 3(x.y&z) Duration 2hrs each direction (total 6 hrs)
6.6 Drop test Height 100cm (to 10mm thickness woodenboard) Direction 3(x.y&z)
6.7 Solderability Test Soldering Temperature 255 C Duration 3 sec
6.8 Accelerated Life Test (ALT) Thermal Cycling : Thermal Cycling consists of temperature ramping components for 30 minutes in the Testing oven from -20°C to 70°C. The components are then exposed for 1 hour at The extremes and the cycle is repeated for a total of 15 cycles.. Thermal Soak: Thermal soak consists of exposing a powered unit to 70°C and 85% relative humidity for 45 days.
G
F
E
D
C
Notice: All specifications must be satisfied in this condition.
B
Date: Drawn by:
A
A
Rev.
09/03/11
Date Drawn
汤浩君
Note
56
Checked by: Approved by:
www.be-star.com wu@be-star.com
4
09/03/11
汤浩君 耿
李红元
3
FT-50T-0.87A1W130
Piezo Ceramic Element
BDRG NO: BS/TEY01.228A
2 1
Page:06 of 08
B
A
Page 7
6 5
FT-50T-0.87A1W130
24 3
1
H
H
7.Packing
7.1Packing Drawing
G
products
foam cover
100PCS
foam tray
F
E
label info
G
F
E
D
and shall not be used in whole or in part without its written content
7.2 packing quantity
7.2-a 600pcs per foam tray
This print and information there in are proprietary to Bestar Electronics Industry Co., Ltd.
7.2-b 5 foam trays per carton
7.2-c Total 3000pcs per carton
7.2-d Transducers shall be packaged in suitable low-sulfur .
C
air tight stacking containers to prevent oxidation of the metal disc. corrosion of the silver electrode. And damage during shipment and storage. Cartons shall be stackable to four feet high without damage to transducers.
B
A 09/03/11 汤浩君
A
Rev.
Date
6
Drawn
FT-47T-0.7A1W060
Datecode: XX.XX
Quantity:5000pcs
Date: Drawn by: Checked by:
Note
5
Approved by:
www.be-star.com wu@be-star.com
4
09/03/11
汤浩君 耿
李红元
3
FT-50T-0.87A1W130
Piezo Ceramic Element
DRG NO: BS/TEY01.228A
2
Page:07 of 08
1
D
C
B
A
Page 8
6 5 4 3
FT-50T-0.87A1W130
H
8. History change record
2 1
H
version
G
F
E
D
No.
A
Before After
Change Items
Date
09/03/11
Drawn
汤浩君
Approved
G
李红元
F
E
D
and shall not be used in whole or in part without its written content
This print and information there in are proprietary to Bestar Electronics Industry Co., Ltd.
C
B
Date: Drawn by:
09/03/11
A
A
Rev.
Date
6
汤浩君
Drawn
Note
5
Checked by: Approved by:
www.be-star.com wu@be-star.com
4
09/03/11
汤浩君
李红元
3
FT-50T-0.87A1W130
Piezo Ceramic Element
BDRG NO: BS/TEY01.228A
Page:08 of 08